Chart Showing Damage Depth of Diamond Grind v. Diamond Particle Size |
Checks in Glass Revealed by Etching with Buffered HF |
100 Grit Damage Remaining After 0.0075" Had Been Removed |
READ CONSULTING provides services to industry in the areas of failure analysis, process development and process improvement. Read Consulting is prepared to use its experience and expertise to analyze customers' specific problems.
Chart Showing Damage Depth of Diamond Grind v. Diamond Particle Size |
Checks in Glass Revealed by Etching with Buffered HF |
100 Grit Damage Remaining After 0.0075" Had Been Removed |